The effect of dentine-bonding agents on the microleakage of provisional crowns.
Abstract (Summary)
The use of provisional acrylic crowns is common practice with prosthodontic treatment. Provisional crowns are prone to marginal leakage and poor retention due to weak interim cements. The aim of this study was to assess the effect of the application of two different dentine-bonding agents on the microleakage of provisional crowns.