Vertikale Wanderwellenmodulatoren auf Quantenfilmbasis für die optische Informationsverarbeitung - Vertical travelling-wave modulators using quantum-well material for optical information processing
Abstract (Summary)
The vertical optical travelling-wave modulator represents a new high-frequency element for optical data processing. The modulator is designed for a wavelength of 1200 nm and combines the layered structure of vertical optical modulators based on pseudomorphic InGaAs/GaAs quantum-wells with microwave lines from the MMIC technology. The quantum confined Stark effect is used to modulate the optical signal. The multiple quantum-well structure is embedded into an asymmetrical Fabry-Perot resonator built from a Bragg reflector and an aluminum layer to increase the electrooptical effect. The modulators produces a reflectivity change of 0,28. Large scale travelling-wave modulators are capable of critical frequencies higher than 40 GHz. By varying the width of the central conductor of the microwave line, the slow-wave factor could be varied experimentally between 4.8 and 12,7. The applied microwave produces a modulation lattice along the microwave line which can be used in a high frequency beam-steering element for optical information processing
Bibliographical Information:
Advisor:Prof. Dr. P. Laws; Prof. Dr. D. Jäger
School:Universität Duisburg-Essen, Standort Essen
School Location:Germany
Source Type:Master's Thesis
Keywords:elektrotechnik gerhard mercator universitaet
ISBN:
Date of Publication:10/12/2001