A Tunable Emission Prepared by Novel Photo-induced Color-Change Materials
Abstract (Summary)
In this thesis , we studied a green emitter (C545T) dopanted SU8. C545T is an organic dye.
[10-(2-benzothiazolyl)-1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H,11Hbenzo[l]-pyrano[6,7,8-ij]quinolizin-11one(C545T)] .
When the sample of C545T and SU8 with thin films were exposured to UV-light. We found that the thin film between with UV exposure (L1-Red) and without UV exposure (L2-Green) will show the different chemistry properties.We can achieve proper CIE coordinates and color by adjusting .The different concentrations of C545T dopanted in SU8 thin films.The L1 and L2 were close-kint blue back-light in order to achieve a tunable emission module . If we crafted meticulously optimization , we can find a exclusive
white light. This is a optic thin film attach to Color-change materials
Bibliographical Information:
Advisor:Yu-Kai Han; Mei-Ying Chang; Ping-Tsung Huang; Wen-Yao Huang
School:National Sun Yat-Sen University
School Location:China - Taiwan
Source Type:Master's Thesis
Keywords:organic color change materials
ISBN:
Date of Publication:01/31/2008