Time-dependent crack growth and fracture in concrete
Abstract (Summary)
The objectives of this thesis are to study time-dependent fracture behaviour in concrete. The thesis consists of an experimental study, constitutive modelling and numerical analysis.
Bibliographical Information:
Advisor:
School:Lunds universitet
School Location:Sweden
Source Type:Doctoral Dissertation
Keywords:TECHNOLOGY; deformationer; betong; brottmekanik; sprickor; sprickbildning; sprickmodeller; krypning; spänningar; brottenergi; brottspänningar; beräkningsmodeller; finita element; teori; laboratorieförsök; tidsberoende; creep rupture; Fictitius Crack Model; finite element method; time-dependent fracture; visco-elastic fracture; sustained loading; rupture test; creep; fracture mechanics; creep crack growth; concrete; tensile fracture; crack model