Synthesis and applications of functionalized pyridinyl imine complexes of palladium.
Abstract (Summary)
-diimine Pd(II) complexes having a functionalized hydrocarbon attached to the imino nitrogen was performed. The catalytic activity of these complexes were then evaluated in the polymerization of ethylene and in the Heck coupling reaction of methyl acrylate with iodobenzene.Unconjugated β
Bibliographical Information:
Advisor:
School:University of the Western Cape/Universiteit van Wes-Kaapland
School Location:South Africa
Source Type:Master's Thesis
Keywords:palladium organopalladium compounds organometallic synthesis
ISBN:
Date of Publication:01/01/2005