Synthesis and Raman scattering studies of novel semiconductor nanostructures [electronic resource] : Si, Ge and GaAs twinning superlattice nanowires /
Abstract (Summary)
The full text of the dissertation is available as a Adobe Acrobat .pdf file (235 p.) ; Adobe Acrobat Reader required to view the file.
Bibliographical Information:
Advisor:
School:Pennsylvania State University
School Location:USA - Pennsylvania
Source Type:Master's Thesis
Keywords:phonon confinement quantum twinning superlattice nanowires raman scattering fano interference semiconductor nanostructures pulsed laser vaporization plv synthesis oxidation