Solid-state ¹³C-NMR investigation of di- and tri-block biodegradable copolymers isolated in their inclusion compounds with cyclodextrins
Abstract (Summary)
PORBENI, FRANCIS EBIKEFE. SOLID-STATE 13C-NMR INVESTIGATION OF
DI- AND TRI-BLOCK BIODEGRADABLE COPOLYMERS ISOLATED IN THEIR
INCLUSION COMPOUNDS WITH CYCLODEXTRIN. (Under the direction of Prof.
Alan E. Tonelli.)
We have synthesized and characterized two biodegradable copolymers: poly(?caprolactone)-poly(L-lactide),
(PCL-b-PLLA) diblock copolymer, and poly(?caprolactone)-poly(propylene
glycol), (PCL-PPG-PCL) triblock copolymer. The lengths
of each block in the diblock were determined to be: PCL = 92 and PLLA = 84. While in
the tri-block, each PCL block length was found to be 45, and the PPG was 60. Inclusion
compounds (ICs) of these copolymers with ?- and ?- cyclodextrins (CDs) were formed
and characterized. The solid crystals of the ICs were found to be in the channel packing
mode, allowing the copolymers to be isolated as straight chains within the cylindrical
channels of the CDs. We have investigated the conformations and dynamics of the
isolated di- and triblock copolymer chains entrapped within the channels of ?- and ?-
cyclodextrins (CD) using solid-state 13C-NMR techniques. The PCL block chains
isolated within the cavities of ?- and ?-CDs, adopt a conformation similar to that of PCL
crystalline blocks in the bulk semi-crystalline di- and tri-block copolymers. The spinlattice
relaxation time T1C measurements confirmed the semi-crystalline morphology of
both of these copolymers. A dramatic difference was observed in the mobility of the
polymer chains in the bulk compared to the ICs. In the absence of intermolecular
interactions, the isolated chains experienced increased mobility relative to their behavior
in the bulk. This result reflects the role of cooperative interactions between the polymer
chains in both the bulk di- and tri-block copolymers. The length scale of proton spin
diffusion was probed using T1H and T1?H. T1H in the bulk copolymers averaged to a single
value, while the T1?? indicated that the copolymers were phase-separated. In the ICs,
exchange of proton magnetization through spin diffusion was observed between the
polymer chains and the CDs, but it was not complete. Two-dimensional solid-state
heteronuclear correlation method was also employed to monitor proton communication in
these samples. Intra-block exchange of proton magnetization was observed in the bulk
copolymers at short mixing times. In the ICs, intra-block 1H-1H spin communication was
observed for the isolated chains. In spite of the physical closeness between the isolated
chains and CD molecules, efficient proton spin diffusion was not observed.
SOLID-STATE 13C-NMR INVESTIGATION OF DI- AND
TRI-BLOCK BIODEGRADABLE COPOLYMERS
Bibliographical Information:
Advisor:
School:North Carolina State University
School Location:USA - North Carolina
Source Type:Master's Thesis
Keywords:north carolina state university
ISBN:
Date of Publication: