Self-assembly of nanomaterials into films and fibers using genetically engineered viruses
Abstract (Summary)
Supervisors: Angela M. Belcher and David A. Vanden Bout. Vita. Includes bibliographical references. Also available from UMI.
Bibliographical Information:
Advisor:
School:The University of Texas at Austin
School Location:USA - Texas
Source Type:Master's Thesis
Keywords:self assembly chemistry nanostructured materials recombinant viruses