Rock alteration and vein mineralization at the Buffalo Mine, Grant County, Oregon
Abstract (Summary)
Master files scanned at 600 ppi (24-bit Color and 256 greyscale) using Capture Perfect 3.0 on a Canon DR-9080C in TIF format. PDF derivative scanned at 300 ppi (24-bit Color and 256 greyscale and 256 B&W), using Capture Perfect 3.0, on a Canon DR-9080C. CVista PdfCompressor 4.0 was used for pdf compression and textual OCR.
Bibliographical Information:
Advisor:
School:Oregon State University
School Location:USA - Oregon
Source Type:Master's Thesis
Keywords:rocks petrology oregon grant county
ISBN:
Date of Publication:06/13/1958