Reactivity and Structure of Supported Nickel Phosphides (Ni2P) in Deep Hydrodesulfurization Catalysis
Abstract (Summary)
This dissertation describes preparation and characterization of Ni2P catalysts and their application in deep hydrodesulfurization (HDS) of a model sulfur compound, 4,6-dimethyldibenzothiophene (4,6-DMDBT), one of the most refractory S-compounds. This topic is of great importance in addressing recently enacted environmental regulations limiting the sulfur content in fuels. The work carried out includes synthesis of Ni2P on different siliceous supports, SiO2, MCM-41, and ultra-stable Y zeolite (USY). It also includes determining the characteristics of the supported Ni2P catalysts with a wide range of techniques: X-ray powder diffraction (XRD), transmission electron microscopy (TEM), Fourier transform infrared (FTIR) and X-ray absorption fine structure (XAFS) spectroscopy. The use of these techniques allowed better understanding of the nature of the active sites as well as the effect of supports. Activity tests were conducted in the HDS of 4,6-DMDBT and the HDN of quinoline. The performance of the catalysts will be compared to that of a conventional sulfide hydrotreating catalyst, Ni-Mo-S/Al2O3. Investigation of the reaction mechanism in the hydrodenitrogenation (HDN) of 2-methylpiperidine together with in situ FT-IR measurements were conducted to understand how catalyst properties affect activity and selectivity.
Bibliographical Information:
Advisor:Rickey M. Davis; Amadeu K. Sum; Brian E. Hanson; S. Ted Oyama; David F. Cox
School:Virginia Polytechnic Institute and State University
School Location:USA - Virginia
Source Type:Master's Thesis
Keywords:chemical engineering
ISBN:
Date of Publication:01/26/2005