Reactions of Group V metal oxide cluster ions insight into heterogeneous catalytic mechanisms /
Abstract (Summary)
Experiments were conducted on the reactions between vanadium and niobium oxide
cluster cations and various hydrocarbon gases in an effort to obtain information on the active sites
on catalytic surfaces. The data acquired may be of use to determine elementary steps in a larger
catalytic mechanism. This provides information on the sites necessary for the promotion of the
desired process as well as on the sites which can either prohibit the desired process or encourage
the generation of unwanted side products.
The guided ion beam mass spectrometer used in these studies allows for the individual
analysis of clusters to determine the conditions required for a desired process. These results are
part of an on-going study to systematically investigate the Group V metal oxide cluster ions
toward hydrocarbons of interest to the catalytic community.
The experiments discussed herein include a variety of reactant gases from saturated
hydrocarbons to aromatic molecules. These studies provide a sampling of the power of this
technique to evaluate different systems. These will be briefly summarized below.
The reactions between the Group V metal oxides with the C2 hydrocarbons, ethane and
ethylene, conducted previously have shown a dramatic preference of the (V2O5)1-3+ clusters to
transfer an oxygen atom to the hydrocarbon. We were unable, however, to determine the neutral
product generated by experimental means. Therefore, we formed a collaboration with a
theoretical group in Berlin, to ascertain the most probable product energetically. Density
functional calculations showed the structures of the two reactive clusters, V2O5+ and V4O10+, both
exhibited an oxygen centered radical moiety as part of their structure which was not observed
with any other cluster studied. It was also determined that acetaldehyde was the preferred
product when (V2O5)1,2+ reacted with ethylene. The calculations also showed that the reactions
with ethane showed that it was energetically possible for V2O5+ to dehydrogenate ethane to yield
ethylene and to proceed further to eventually give acetaldehyde as a neutral product.
iii
A second study discussed here involves the reactions between the vanadium and niobium
oxide cluster cations with methanol. Methanol is of interest industrially as an alternate fuel
source. Hence, any information one may obtain to improve the selectivity and overall efficiency
is of vital interest. Certain clusters demonstrated the association of molecular hydrogen. This
was determined using deuterated methanol. These products were also observed under single
collision conditions with the only possible mechanism being dehydrogenation of methanol to
yield H2, adsorbed to the cluster, and CH2O, the neutral product. In addition, the association of
C2H6O was also observed. Among the possible structures of C2H6O is dimethyl ether. This is not
the only structure though and additional experiments are required to ascertain the exact structure
on the cluster.
The reactions between vanadium and niobium oxide cluster cations and propylene were
also investigated. The polyolefin industry is a considerable part of the economy itself as well as
producing precursors to several other substances. The oxidation of propylene is also a useful
process, generating products such as propylene oxide. Considering the closeness in structure
from propylene to ethylene, there was hope that the Group V metal oxide clusters would also
show a significant oxygen transfer pathway for the propylene. The reactions between the
vanadium and niobium oxide cluster cations mainly consisted of the formation of the monomer
and dimer and even went as high as the pentamer. The addition of methyl and ethyl groups to the
monomer and dimer were also observed. The oxygen transfer from the metal oxide cluster to the
propylene was also noted for V2O5+ and Nb2O5+ but not for V4O10+. The reactivity was greater for
the V2O5+ than for the Nb2O5+, however this is to be expected since the V-O bond is more easily
cleaved than the Nb-O bond.
The last study included here involves the reactions between the vanadium and niobium
oxide cluster cations with ortho-xylene. Xylene is of interest in the production of phthalic
anhydride which is used to produce polyester resins and polyvinylchloride. Xylene is also worth
studying to determine if the methyl groups affect the reactivity with the metal oxide cluster ions.
iv
The V2O5+ cluster was the only species to exhibit an oxygen transfer pathway. The majority of
the products observed were charged hydrocarbons. Among these were the production of C7H7+,
the loss of a methyl group, C8H10+, charge transfer, C8H10CH3+, addition of a methyl group to the
charged xylene molecule, and (C8H10)2CH3+ and (C8H10CH3)2+, single and double methyl addition
to the xylene dimer, respectively. Select clusters also exhibited the association of the C7H7 and
C8H10 species.
v
Bibliographical Information:
Advisor:
School:Pennsylvania State University
School Location:USA - Pennsylvania
Source Type:Master's Thesis
Keywords:
ISBN:
Date of Publication: