Preparation and reactions of Diels-Alder adducts of lignin-derived quinones
Abstract (Summary)
PERSPECTIVE
THESIS OBJECTIVES
BACKGROUND
Characteristics of Quinone Pulping Catalysts
Conversion of Lignin and Lignin-Related Compounds
to Quinones
Thermal/Chemical Modifications
Chemical Modifications
Potassium Nitrosodisulfonate (Fremy's Salt)
Sodium Periodate
Hydrogen Peroxide
Peracetic Acid
Other Chemical Reactions
Summary
Electrochemical Modifications
Biochemical Modifications
Modification and Stabilization of Quinones
The Diels-Alder Reaction
Modification of p-Quinones
Modification of o-Quinones
Bibliographical Information:
Advisor:
School:Georgia Institute of Technology
School Location:USA - Georgia
Source Type:Master's Thesis
Keywords:institute of paper science and technology
ISBN: