Open-Framework Germanates : Crystallography, structures and cluster building units
Abstract (Summary)
This thesis is focussing on the crystallographic challenges and what knowledge we can gain from studying the different open-framework germanates. Five new open-framework germanates have been synthesized and the structures have been determined by single crystal X-ray diffraction. A thorough description is made of the different problems raised with the different compounds, whether it is choice of crystal system in SU-61, twinning and possible ordering in SU-46, superstructure and variation in elemental content in SU-57, template disorder in JLG-5 or framework disorder in SU-44.Open-framework germanates are often built from one type of cluster, such as the Ge7 [Ge7X19], Ge8 [Ge8X20], Ge9 [Ge9Xn, n =25-26] and Ge10 [Ge10X28], (X =O, OH, F) clusters. The structures built by clusters containing different kinds of polyhedra are discussed, with a focus on the 4-coordinated Ge7 clusters, the larger cluster aggregate found in SU-8 and SU-44 and the structures built by the Ge10 clusters.
Bibliographical Information:
Advisor:
School:Stockholms universitet
School Location:Sweden
Source Type:Doctoral Dissertation
Keywords:NATURAL SCIENCES; Chemistry; germanate; crystallography; building unit; zeotype; scale chemistry; Structural Chemistry; strukturkemi
ISBN:978-91-7155-570-0
Date of Publication:01/01/2008