Nonlinear spin dynamics and ultra-fast precessional switching [electronic resource] /
Abstract (Summary)
Title of Dissertation: NONLINEAR SPIN DYNAMICS AND
ULTRA-FAST PRECESSIONAL SWITCHING
Mihai Dimian, Doctor of Philosophy, 2005
Dissertation directed by: Professor Isaak D. Mayergoyz
Department of Electrical and Computer Engineering
This thesis is intended to provide a theoretical analysis of magnetization dynamics in
nanometer scale structures over picosecond time scales. This research has been
motivated by promising technological applications in the area of magnetic data
storage, as well as by pure scientific quest for ultra-fast spin dynamics in
nanostructures.
The present paradigm of magnetic data storage is approaching its fundamental
limits for areal storage density, as well as for speed in data processing. As a result,
there is an urgent need for reliable alternatives to current magnetic recording media,
which are based on longitudinal thin film, and to the conventional mechanism of
magnetization reversal, based on damping switching. In this dissertation, faster
modes of magnetization reversals, using precessional magnetization motion, are
analyzed in traditional longitudinal media and in its promising alternatives:
perpendicular and patterned media. This analysis uses multi-spin description of
magnetic nanoparticles and continuum micromagnetics for thin film media. The
spins dynamics in both discrete and continuum versions is modeled by Landau
Lifshitz type equations. These models are introduced in Chapter 2, subsequent to an
overview of magnetic recording media offered in Chapter 1.
The analytical study of precessional switching in perpendicular thin film media
is presented in Chapter 3. The features of precessional magnetization switching and
conventional magnetization reversal are compared, and the design of magnetic field
pulses that guarantee precessional switching is discussed. In Chapter 4, the study of
precessional magnetization switching in longitudinal thin film media is undertaken.
After a short summary of the research studies on this topic, the inverse problem
approach to the analysis of precessional switching in these media is presented. This
approach leads to explicit expressions for the magnetic field pulses that guarantee the
precessional switching.
The study of surface anisotropy effects on magnetization reversals in
nanoparticles is presented in Chapter 5. The expressions for critical magnetic fields
that guarantee the quasi-static and precessional reversals are analytically derived for
the case of very strong exchange and weak surface anisotropy. These analytical
results are also used to test the numerical approach, which is applied to the general
case of the problem.