Nondestructive evaluation of loading and fatigue effects in HAYNES 230 alloy
Abstract (Summary)
Nondestructive evaluation is a useful method for studying the effects of
deformation and fatigue. In this dissertation I employed neutron and X-ray
diffraction, nonlinear resonant ultrasound spectroscopy (NRUS), and infrared
thermography to study the effects of deformation and fatigue on two different
nickel based superalloys. The alloys studied were HAYNES 230, a solid solution
strengthened alloy with 4% M6C carbides, and secondarily HASTELLOY C-2000
a similar single phase alloy.
Using neutron and X-ray diffraction, the deformation behavior of