New Series of Photoluminescent Polymers Containing 3,4-diphenylthiophene and 1,4-di(1,3,4-oxadiazolyl)phenylene
Abstract (Summary)
We plan to prepare conjugated polymers containing £k-excessive thiophene and £k-deficient oxadiazole group in the main chain, and introduction of phenyl or alkoxy groups on the side chain. The NMR, IR, TGA, DSC, GPC, stability, and other optical properties will be examined.
Bibliographical Information:
Advisor:Yun-Long Hong; Jin-Long Hong; Tsu-Hsin Chang
School:National Sun Yat-Sen University
School Location:China - Taiwan
Source Type:Master's Thesis
Keywords:photoluminescent quantum efficiency conjugated polymer
ISBN:
Date of Publication:07/03/2003