NMR imaging of curing processes

by Erich, Sebastiaan Joannes

Abstract (Summary)
Title from title screen (viewed on Dec. 6, 2007). Title from document title page. Includes bibliographical references. Available in PDF format via the World Wide Web.
Bibliographical Information:

Advisor:

School:Technische Universiteit Eindhoven

School Location:Netherlands

Source Type:Master's Thesis

Keywords:nuclear magnetic resonance alkyd resins coatings