Hydrophobic and hydrophilic control in polyphosphazene materials

by 1979- Steely, Lee Brent

Abstract (Summary)
iii This thesis is the culmination of several recent studies focused on the surface characterization of polyphosphazenes specifically the properties of water repellency or hydrophobicity. Chapter 1 is a background account of polyphosphazene chemistry and the hydrophobicity of polyphosphazenes.