Fracture toughness evaluation of testing procedure to simplify J [subscript Ic] calculations /
Abstract (Summary)
The purpose of this study is to examine the current fracture toughness test
procedure and to determine if there is an easier, less complicated method to get the JIc
value from a test record for fracture toughness specimens. The current method for
constructing JIc is complicated and involves a detailed computer program or spreadsheet.
The objective in this study is to simplify the analysis for the determination of JQ.
This study has shown that the load and displacement record for a fracture
toughness specimen can be used to directly estimate a JQ value, a provisional value for
fracture toughness, JIc. The maximum load point is used along with an adjustment factor
for this direct estimation of the JQ value. This JQ value is equivalent to that obtained from
the construction procedure, when a unit-sized specimen is tested, that is, a specimen with
a width of 50 millimeters (2 inches) and a thickness of 25 millimeters (1 inch). Other
sizes require a size adjustment factor, which is simply a function of the specimen width
relative to the unit width. The adjustment factor proposed is a square root relationship
between the width of the test specimen and a unit width. This shows that the effort
required for the proposed new method of constructing JIc is less than that required for the
construction method, the new method is simple in concept and requires a minimum
number of calculations, and the method appears to produce values of JQ which are
comparable to those obtained from the construction procedure and may have less inherent
scatter.
iv
Bibliographical Information:
Advisor:
School:The University of Tennessee at Chattanooga
School Location:USA - Tennessee
Source Type:Master's Thesis
Keywords:
ISBN:
Date of Publication: