Faseroptische Multi-Fabry-Perot-Sensoren in Schichtbauweise
Abstract (Summary)
This work deals with fiber-optic sensors for measuring pressure und temperature by using the fabry-perot-effect. The realised sensors are made of polymer thin-films with special reflection-coatings. The special kind of sensor takes part in the group of senors in reflection mode transmission mode is possible.