Direkte Bestimmung von Eisenspuren in Dichlorsilan mit Hilfe der Graphitrohrofen-Atomabsorptionsspektrometrie (GF-AAS) - Direct Determination of Trace Amounts of Iron in Dichlorosilane by Graphite Furnace Atomic Absorption Spectrometry (GF-AAS)
Abstract (Summary)
In the present thesis the development of an analytical method for the determination of trace amounts of iron in dichlorosilane by graphite furnace atomic absorption spectrometry with a modified autoprobe unit is described. An conceived gas inlet system enabled a nearly contamination free and constant gas injection. The analytical method is optimized and the iron concentration in dichlorosilane is quantitatively determined.