DEVELOPMENT OF NEXT GENERATION CARPET BACKINGS FOR FACILE RECYCLABILITY
Abstract (Summary)
The overall goal of the research was to develop the next generation, generic
construction of broadloom carpet that will compete on both a performance and cost basis
with the current construction while avoiding the major recycling disadvantages of the
latter. The new construction was designed to maintain nearly all of the current carpet
formation processes to minimize capital investment in converting existing manufacturing
lines. A major industry constriction was that the new construction must at least meet the
current construction's physical performance on the floor and overall cost characteristics.