Heat treatment can be defined as a combination of heating and cooling operations applied
to a metal or alloy in solid state. It is an important manufacturing process, which controls
the mechanical properties of metals, therefore contributes to the product quality.
Computerized Heat Treatment Planning System for Quenching and Tempering (CHTq/t),
a windows based stand alone software, is developed to assist the heat treatment
process design. The goal of CHT-q/t is to predict the temperature profile of load in batch
as well as continuous furnace during heating, quenching and tempering of steel, then to
predict the mechanical properties as Quenched
&
Tempered, and finally to optimize the
heat treatment process design.
The thesis reviews existing heat treating simulation software and identifies the industrial
need of a software tool which integrates part load and furnace model with heat treating
process. The thesis discusses cooling curve of specimen and Time Temperature
Transformation (TTT) diagram to determine the microstructure evolution and
subsequently the mechanical properties of steel after quenching. An extensive database
has been developed to support the various function modules. The thesis focuses mainly in
the TTT and quenchant database development, property prediction after quenching and
tempering and the implementation of software. The properties determined in the thesis
are hardness, ultimate tensile strength, yield strength, toughness and percentage
elongation. Hardness has been predicted by the use of some well known analytical
equations and the TTT database, finally regression analysis has been used to give the
value as a function of carbon percentage and volume fraction of martensite. The other
mechanical properties are calculated based on a relation of hardness and volume fraction
of martensite.
Various case studies were performed to show the application of CHT-bf and CHT-cf at
Bodycote Thermal Processing, Worcester
&
Waterbury. The objective behind the case
studies was to study the effect of change in load arrangement, production rate and cycle
time on the heat treated parts and finally to give recommendations in order to save energy
and improve productivity and quality.
ii
Bibliographical Information:
Advisor:
School:Worcester Polytechnic Institute
School Location:USA - Massachusetts
Source Type:Master's Thesis
Keywords:metals tempering
ISBN:
Date of Publication: