Development of computer aided heat treatment planning system (CAHTPS)
Abstract (Summary)
The thesis includes fundamental work in the following,
•
Development of materials database which includes the main parameters of the various
heat transfer models
•
Validation and testing of the system capability and accuracy by means of various case
studies
A computer aided heat treatment planning system (CAHTPS) is developed to
assist the heat treatment process. The temperature distribution inside the furnace and the
temperature of the various parts in the load can be determined. The various models for
the heat treatment are analyzed and the various parameters in the equations are classified.
The majority of the equations parameters were properties of various metals and non
metals. Hence an extensive database is developed so as to assist the models.
The remaining physical conditions dependent parameters of the models were
analyzed and the effects due to change in the conditions and these parameters are tested
and studied by various case studies. The change in the loading pattern effects and change
in the load quantity effects for the various cases are presented.
The thesis work establishes the system’s application scope and the accuracy to be
used in the current heat treatment industries.
i
Bibliographical Information:
Advisor:
School:Worcester Polytechnic Institute
School Location:USA - Massachusetts
Source Type:Master's Thesis
Keywords:metals
ISBN:
Date of Publication: