Characterization of as-grown and annealed narrow band gap nitrides grown by molecular beam epitaxy
Abstract (Summary)
Supervisor: Archie L. Holmes, Jr. Vita. Includes bibliographical references. Also available from UMI.
Bibliographical Information:
Advisor:
School:The University of Texas at Austin
School Location:USA - Texas
Source Type:Master's Thesis
Keywords:nitrides molecular beam epitaxy optoelectronic devices