Analytical modeling of fully bonded and debonded pre-tensioned prestressed concrete members

by 1963- Baxi, Asit Nareshchandra

Abstract (Summary)
Supervisors: Sharon L. Wood and Ned H. Burns. Vita. Includes bibliographical references. Also available from UMI.