Analysis of in-cavity thermal and pressure characteristics in aluminum alloy die casting
Abstract (Summary)
The lack of effective control of the die casting process is the primary reason for the occurrence of defective die cast products. A reliable process control system must be capable of measuring the process variables, comparing them to the standard or ideal values and making suitable alterations in the process to eliminate any deviation from the ideal. This study attempted to facilitate the development of such a process control system. A two pronged approach was used to achieve this objective. The experimental approach addressed some of the problems in the measurement of process variables. The analytical approach addressed some of the problems in the design of the process and subsequent identification of the ideal process variable values. The experimental approach concentrated on the measurement of in-cavity pressure and thermal characteristics of the die casting process. Kistler direct pressure sensors were evaluated and utilized for cavity pressure measurement during the die casting campaign...
Bibliographical Information:
Advisor:
School:The Ohio State University
School Location:USA - Ohio
Source Type:Master's Thesis
Keywords:
ISBN:
Date of Publication:01/01/1996